MAGMAWELD ENi99 4.0mm Cast Iron Nickel Stick Electrodes 10KG
$1,399.00
Product Description
Magmaweld ENi99 is a premium 99% nickel cast iron stick electrode, ideal for low/medium phosphorus cast iron repairs. Features easy arc striking, stable arc, and machinable weld metal. Suitable for steel/copper/nickel to cast iron joining, with single pass welds recommended.
Specifications
| Nickel Content | 99% |
| Diameter | 4.0mm |
| Length | 400mm |
| Weight | 10kg (¡Ö200 sticks) |
| Standards | AWS SFA-5.15, EN ISO 1071 |
MAGMAWELD ENi99 – Cast Iron Nickel 4.0mm Stick Electrodes – 10KG Pack
Core Specifications
| Nickel Content | 99% |
| Diameter | 4.0mm |
| Length | 400mm |
| Pack Weight | 10kg (~200 sticks) |
| Preheating Requirement | Max. 300¡ãC |
| Hardness (HB) | 160 (as welded) |
| Welding Position | PA, PB, PC, PD, PE, PF |
| Polarity | DCEP (AC compatible) |
| Standards | AWS/ASME SFA-5.15, EN ISO 1071 |
| Re-drying Cycles | Max. 5 times (350¡ãC for 2 hours) |
Why Choose ENi99?
Premium 99% nickel electrodes deliver exceptional strength for critical cast iron repairs. The high nickel content ensures superior weld integrity compared to 55% nickel alternatives, making it ideal for low/medium phosphorous castings. Experience easy arc striking, stable performance, and machinable weld deposits¡ªperfect for single-pass repairs and dissimilar material joining (steel/copper/nickel to cast iron).
Applications
Engineered for welding lamellar graphite, white/black heart malleable, and nodular cast iron. Ideal for repairing cracked cast iron components in automotive, industrial machinery, and heavy equipment. Suitable for both fabrication and maintenance welding across all positions (flat to overhead).
Performance Highlights
– Low preheating requirement minimizes distortion
– Smooth bead surface with reduced spatter
– Hammer peening capability reduces residual stress
– Excellent crack resistance on high-stress components
– Consistent mechanical properties (160 HB hardness)
Quality Assurance
Manufactured by market-leading Magmaweld to international standards (AWS/EN ISO). Each 10kg pack undergoes strict quality control, ensuring industrial-grade performance for professional welding applications.
FAQ
– Can ENi99 be used on high-phosphorus cast iron? Best results on low/medium phosphorous castings.
– Is post-weld heat treatment required? Not mandatory, but hammer peening recommended before cooling.
– What’s the shelf life? Store in dry conditions; re-dry up to 5 times at 350¡ãC for 2 hours if exposed to moisture.
Ready to Upgrade Your Welding Repairs?
For bulk pricing, technical support, or custom packaging options, contact our team today. Experience the Magmaweld difference in cast iron welding performance.